P + S
Reaction P + S PS(n)
Phase transition


ReagentP(red phosphorus) coarse powder

S powder (6N)
CompanyRare Metallic Co. Ltd.
Weight19.7mg
ContainerAl pan, treated in N2 atmosphere
Comment
Figure shows only the first heating process. Sulfidation reaction starts at 180, and continues till 325. Peak at 219.
H=506.7J/g.
The enthalpy of formation
@Product is unstable in air. Very hygroscopic. Decomposition was accompanied by the evolution of H2S gas.